Patents for C30B 7 - Single-crystal growth from solutions using solvents which are liquid at normal temperature, e.g. aqueous solutions (3,917)
05/1977
05/17/1977US4024013 Thermosensitivity
05/03/1977US4021294 Growing quartz crystals, exposure to ionizing irradiation
04/1977
04/26/1977US4019950 Hydrothermal; lead carbonate from the carbonate or basic carbonate; alkali metal bicarbonate
01/1977
01/18/1977US4003757 Silver-II-oxide for galvanic elements
11/1976
11/16/1976US3992197 Silver crystals and production thereof
09/1976
09/21/1976US3981973 Metal salts
08/1976
08/24/1976US3976535 Hydrothermal
07/1976
07/27/1976US3971876 Temperature control apparatus
07/13/1976US3969182 Growth of mercuric iodide single crystals from dimethylsulfoxide
06/1976
06/01/1976US3961105 Method for the manufacture of coated calcium sulfate whisker fibers
06/01/1976US3960501 Apparatus for growing crystals from hydrothermal solutions
05/1976
05/25/1976US3959453 Lead dioxide
05/18/1976US3957604 Electrolysis
05/18/1976US3957504 Metals, chelate compounds
04/1976
04/06/1976US3949323 Crystals of (K, Rb, NH4)TiO(P, As)O4 and their use in electrooptic devices
03/1976
03/02/1976US3941648 Crystal growth on Hg3 TeO6
02/1976
02/03/1976US3936276 Process for producing amethyst crystal
1 ... 30 31 32 33 34 35 36 37 38 39 40